K2324 Blue-Grey
K2324 Blue-Grey
Firing range 920 - 1300°C. K2324=32/4
Upper piece fired at 1020°C and lower at 1250°C.
Molemmissa lasitepohjana on kirkas laajapolttoinen 921 lasite ja pigmenttiä lisätty 8%. 
from
20,20 €
K8553 Black
K8553 Black
Firing range 920 - 1300°C.
Very Black! K8553=55/3
Chemical composition Cr-Co-Fe-Ni... 
from
18,32 €
K4816 Neutral Grey
K4816 Neutral Grey
Firing range 920 - 1300°C. Chemical composition Fe-Cr-Co-Ni. 
from
5,21 €
K2482 Deep Black
K2482 Deep Black
Firing range 920 - 1300°C. Chemical composition Cr-Co-Fe-Ni-Mn
Blue-black tone. 
from
11,58 €
K2890 Deep Grey
K2890 Deep Grey
Firing range 920 - 1300°C. Chemical composition Fe-Cr-Co-Ni. 
from
5,24 €
Underglaze Pencil Light Brown 608
Underglaze Pencil Light Brown 608
Pencils can be used in temperatures 1020 - 1260ºC.
Colours usually darken at higher temperature, but some (usually red tones) start fading. Laitetaan tavallisesti raakapoltetun päälle ja lasitetaan. 
18,50 €
Underglaze Pencil Dark Brown 601
Underglaze Pencil Dark Brown 601
Pencils can be used in temperatures 1020 - 1260ºC.
Colours usually darken at higher temperature, but some (usually red tones) start fading. Laitetaan tavallisesti raakapoltetun päälle ja lasitetaan. 
18,50 €
Underglaze Pencil Red 615
Underglaze Pencil Red 615
Pencils can be used in temperatures 1020 - 1260ºC.
Colours usually darken at higher temperature, but some (usually red tones) start fading. Laitetaan tavallisesti raakapoltetun päälle ja lasitetaan. 
18,50 €
Underglaze Pencil Dark Green 603
Underglaze Pencil Dark Green 603
Pencils can be used in temperatures 1020 - 1260ºC.
Colours usually darken at higher temperature, but some (usually red tones) start fading. Laitetaan tavallisesti raakapoltetun päälle ja lasitetaan. 
18,50 €
Underglaze Pencil Dark Blue 604
Underglaze Pencil Dark Blue 604
Pencils can be used in temperatures 1020 - 1260ºC.
Colours usually darken at higher temperature, but some (usually red tones) start fading. Laitetaan tavallisesti raakapoltetun päälle ja lasitetaan. 
18,50 €
Underglaze Pencil Yellow 605
Underglaze Pencil Yellow 605
Pencils can be used in temperatures 1020 - 1260ºC.
Colours usually darken at higher temperature, but some (usually red tones) start fading. Laitetaan tavallisesti raakapoltetun päälle ja lasitetaan. 
18,50 €
Underglaze Pencil Black 606
Underglaze Pencil Black 606
Pencils can be used in temperatures 1020 - 1260ºC.
Colours usually darken at higher temperature, but some (usually red tones) start fading. Laitetaan tavallisesti raakapoltetun päälle ja lasitetaan. 
18,50 €
Underglaze Pencil Turquoise 609
Underglaze Pencil Turquoise 609
Pencils can be used in temperatures 1020 - 1260ºC.
Colours usually darken at higher temperature, but some (usually red tones) start fading. Laitetaan tavallisesti raakapoltetun päälle ja lasitetaan. 
18,50 €
FK407 Yellow
FK407 Yellow
Firing range 920 - 1300°C. Chemical composition Zr-Si-Pr.
Optimal amount when added to glaze approx. 3 - 6%. 
from
7,00 €
FK 520 Green
FK 520 Green
Firing range 920 - 1350°C. Chemical composition Cr-Co-Si.
Optimal amount when added to glaze approx. 3 - 6%. 
from
6,00 €
FK 4198 Victorian Green
FK 4198 Victorian Green
Firing range 920 - 1300°C. Chemical composition Zr-Si-V-Pr-Co-Ni-Cr-Fe.
Optimal amount when added to glaze approx. 6%. 
from
7,00 €
FK4826 Mint Green
FK4826 Mint Green
Firing range 920 - 1400°C. Chemical composition Zr-Si-Pr-V.
Optimal amount when added to glaze approx. 3 - 6%. 
from
7,10 €
FK560 Light Green
FK560 Light Green
Firing range 920 - 1250°C. Chemical composition Zr-Si-Pr-V.
Optimal amount when added to glaze approx. 6%. 
from
11,00 €
tech
Varnia Oy
Myllypakantie 2
FI-25410, Suomusjärvi
FINLAND
tel. (02) 722 1202
varnia (at) varnia.fi
Business ID: 0202891-2